Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSD11 Normal Grade Heat Sealable Film (thickness: 18 µm)
HSD11 is a general, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dim..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSD11 Normal Grade Heat Sealable Film (thickness: 20 µm)
HSD11 is a general, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dim..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSD11 Normal Grade Heat Sealable Film (thickness: 25 µm)
HSD11 is a general, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dim..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSD11 Normal Grade Heat Sealable Film (thickness: 30 µm)
HSD11 is a general, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dim..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSD12 Normal Grade Heat Sealable Film (thickness: 18 µm)
HSD12 is a printing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona trea..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSD12 Normal Grade Heat Sealable Film (thickness: 20 µm)
HSD12 is a printing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona trea..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSD12 Normal Grade Heat Sealable Film (thickness: 25 µm)
HSD12 is a printing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona trea..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSD12 Normal Grade Heat Sealable Film (thickness: 30 µm)
HSD12 is a printing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona trea..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 18 µm)
HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 20 µm)
HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 25 µm)
HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 30 µm)
HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSS11 Normal Grade Heat Sealable Film (thickness: 18 µm)
HSS11 is a general, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimens..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSS11 Normal Grade Heat Sealable Film (thickness: 20 µm)
HSS11 is a general, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimens..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSS11 Normal Grade Heat Sealable Film (thickness: 25 µm)
HSS11 is a general, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimens..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSS11 Normal Grade Heat Sealable Film (thickness: 30 µm)
HSS11 is a general, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimens..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSS12 Normal Grade Heat Sealable Film (thickness: 18 µm)
HSS12 is a printing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona treatme..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSS12 Normal Grade Heat Sealable Film (thickness: 20 µm)
HSS12 is a printing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona treatme..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSS12 Normal Grade Heat Sealable Film (thickness: 25 µm)
HSS12 is a printing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona treatme..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSS12 Normal Grade Heat Sealable Film (thickness: 30 µm)
HSS12 is a printing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona treatme..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSS13 Normal Grade Heat Sealable Film (thickness: 18 µm)
HSS13 is a metalizing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has coron..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSS13 Normal Grade Heat Sealable Film (thickness: 20 µm)
HSS13 is a metalizing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has coron..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSS13 Normal Grade Heat Sealable Film (thickness: 25 µm)
HSS13 is a metalizing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has coron..
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Kinlead HSS13 Normal Grade Heat Sealable Film (thickness: 30 µm)
HSS13 is a metalizing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has coron..
Copyright © lookpolymers.com All Rights Reserved