Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.0640 GPa | 9.28 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer The Tritheva TN 2020 resin is a Ethylene-Vinyl Acetate copolymer (EVA) developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Th.. |
|||
Secant Modulus, TD | 0.0640 GPa | 9.28 ksi | 50 µm (2 mil) film; ASTM D882 |
DuPont Elvax® 3135SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 12 wt% Vinyl Acetate.Elvax® 3135SB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |