Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 4.14 GPa | 600 ksi | ASTM D882 |
Total PPH 3271 Polypropylene, Oriented Film Extrusion Grade Homopolymer film gradeLow Residuals – FINA 3271 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock –.. |
|||
Secant Modulus, TD | 4.14 GPa | 600 ksi | ASTM D882 |
Total PPH 3371 Polypropylene, Oriented Film Extrusion Grade Homopolymer film gradeLow Residuals - Fina 3371 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock - Fina.. |
|||
Secant Modulus, TD | 4.14 GPa | 600 ksi | ASTM D882 |
Total PPH 3276 Polypropylene, Oriented Film Extrusion Grade Homopolymer film gradeLow Residuals – Fina 3276 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock .. |