Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.0440 GPa | 6.38 ksi | 50 µm (2 mil) film; ASTM D882 |
DuPont Elvax® 3165 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3165 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Secant Modulus, TD | 0.0440 GPa | 6.38 ksi | 50 µm (2 mil) film; ASTM D882 |
DuPont Elvax® 3170SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3170SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res.. |
|||
Secant Modulus, TD | 0.0440 GPa | 6.38 ksi | 50 µm (2 mil) film; ASTM D882 |
DuPont Elvax® 3173SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
(discontinued **)< 18 wt% Vinyl Acetate.Elvax® 3173SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res.. |