Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.380 GPa | 55.1 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® TD-9055-E Hexene LMDPE Film Resin Excellent stiffness and glossApplications: Diaper back sheet, BlendingAdditives: High temperature AOFilm properties are typical of cast film extruded at 280°C.Information provided by NOVA Chemicals.. |
|||
Secant Modulus, TD | 0.380 GPa | 55.1 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® TF-0338-E Hexene LMDPE Film Resin Excellent stiffness and glossApplications: Diaper back sheet, BlendingAdditives: High temperature AOFilm properties are typical of film extruded at 280°C.Information provided by NOVA Chemicals. |
|||
Secant Modulus, TD | 0.380 GPa | 55.1 ksi | ASTM D882 |
Huntsman PE1076 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrap packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (.. |
|||
Secant Modulus, TD | 0.380 GPa | 55.1 ksi | ASTM D882 |
Huntsman PE1078 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrap packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (.. |