Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.211 GPa | 30.6 ksi | ASTM D882 |
ExxonMobil Exceed™ 350D60 LDPE/Hexene Tough Premium Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D60 resin have outstanding tensile, impact streng.. |