Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.150 GPa | 21.8 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® TF-0219-E Hexene LLDPE Film Resin Exceptional toughens, Low gel levelApplications: Cast stretch wrapAdditives: High temperature A/OFilm properties are typical of cast film extruded at a melt temperature of 540°F, and a line speed o.. |
|||
Secant Modulus, TD | 0.150 GPa | 21.8 ksi | 1%, Flexural; ASTM D882 |
Braskem Flexus® 9200 LLDPE Blown Film Extrusion Description: Flexus 9200 is a LLDPE hexene copolymer produced through metallocene catalyst which presents excellent impact and puncture strength, beyond a differential sealing performance comparing .. |
|||
Secant Modulus, TD | 0.150 GPa | 21.8 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TS7003 LDPE Blown Film Extrusion Polyethylene TS7003 is a low-density polyethylene (LDPE) with high molecular weight that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily processed. Th.. |
|||
Secant Modulus, TD | 0.150 GPa | 21.8 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TX7003 LDPE Blown Film Extrusion Polyethylene TX7003 is a low-density, high molecular-weight polyethylene that offers high mechanical strength. The product's characteristics allow for high versatility and use in various applications due to its .. |