Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.130 GPa | 18.9 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TS 7001 LDPE - Heavy Duty Low Friction Film The Trithene TS 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and low coefficient of fricti.. |
|||
Secant Modulus, TD | 0.130 GPa | 18.9 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TX 7001 LDPE - High Molecular Weight The Trithene TX 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and environmental stress crac.. |
|||
Secant Modulus, TD | 0.130 GPa | 18.9 ksi | ASTM D882 |
Chevron Phillips 7120ST LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, Cast/Blown Film ResinCharacteristics: Good Drawdown, Can be used in blown or cast applicationsApplications:Stretch Wrap, CoextrusionsProcessing Conditions: Extruder 6.3.. |
|||
Secant Modulus, TD | 0.130 GPa | 18.9 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding.. |
|||
Secant Modulus, TD | 0.130 GPa | 18.9 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TS7010 LDPE Blown Film Extrusion Polyethylene TS7010 is a low-density polyethylene (LDPE) that presents excellent processability and good mechanical properties. The incorporated additives package warrants a low coefficient of friction (COF) all.. |
|||
Secant Modulus, TD | 0.130 - 0.450 GPa | 18.9 - 65.3 ksi | Average value: 0.253 GPa Grade Count:57 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m.. |
|||
Secant Modulus, TD | 0.130 GPa | 18.9 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TS 3003 LDPE - Film Grade The Trithene® TS 3003 resin is a low-density, high molecular weight polyethylene that offers high mechanical strength and excellent optical properties. The product shows high modulus of elasticity,.. |
|||
Secant Modulus, TD | 0.130 GPa | 18.9 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TX 4003 LDPE and LLDPE Blend - High Resistance Film The Trithene® TX 4003 resin is a blend of low-density polyethylene (LDPE) of high molecular weight with linear low-density polyethylene (LLDPE) designed for the production of industrial films. Sinc.. |