Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 1.172 - 1.413 GPa | 170.0 - 204.9 ksi | ASTM D882 |
Honeywell ACLAR® 11A (0.90 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Secant Modulus, TD | 1.172 - 1.413 GPa | 170.0 - 204.9 ksi | ASTM D882 |
Honeywell ACLAR® 11A(0.60 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Secant Modulus, TD | 1.172 - 1.379 GPa | 170.0 - 200.0 ksi | ASTM D882 |
Honeywell ACLAR® 22C (5.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Secant Modulus, TD | 1.172 - 1.38 GPa | 170.0 - 200 ksi | ASTM D882 |
Honeywell ACLAR® UltRx 2000 CTFE Homopolymer, Barrier Film Description: ACLAR® UltRx 2000 is a 2 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipmen.. |