Mechanical Properties Metric English Comments
Secant Modulus, TD 0.105 GPa
15.2 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging
The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength..
Secant Modulus, TD 0.105 GPa
15.2 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film
The Trithene TS 8064 resin is a low-density polyethylene (LDPE) with a medium molecular weight an excellent processability. Furthermore, this product has good mechanical properties, average transpar..