Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.0990 GPa | 14.4 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TS 7045 LDPE - Film - Plastification The Trithene TS 7045 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |