Secant Modulus, TD 0.703 GPa
102 ksi
ASTM D 882 A
Total Finathene® 6450 HDPE film  (discontinued **)
Applications: overwrap, food packaging, coextrusion, extrusion coatingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lin..
Secant Modulus, TD 0.700 GPa
102 ksi
0.05-1.05%; ISO 527-3
Borealis Borstar® FB1460 HDPE for Film
Borstar FB1460 is a high-density polyethylene film grade, which combines superior physical properties with excellent processability. Due to the high density, the material properties are best utiliz..
Secant Modulus, TD 0.703 GPa
102 ksi
ASTM D 882 A
Total 6410 HDPE Film Resin
Unique combination of high stiffness and clarity; Good moisture barrier properties; Good processability; Good compatibility with LDPE and LLDPEApplications: paper overwrap, cup overwrap, plate overw..
Secant Modulus, TD 0.700 GPa
102 ksi
2% Secant Modulus; ASTM-D882
Braskem TN2005 EVA General Film Copolymer
TN2005 is an Ethylene-Vinyl Acetate (EVA) copolymer with high molecular weight, excellent mechanical properties, transparency, high gloss, and easy processing. Additionally, TN2005 has flexibility e..