Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.0712 GPa | 10.3 ksi | Film value |
Dow AFFINITY™ PL 1850 Polyolefin Plastomer AFFINITY® PL 1850 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide blown and cast film products with low temperature sealability, excellent optics and good abuse resistanc.. |