Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 1.172 - 1.413 GPa | 170.0 - 204.9 ksi | ASTM D882 |
Honeywell ACLAR® 11A (0.90 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Secant Modulus, TD | 1.172 - 1.413 GPa | 170.0 - 204.9 ksi | ASTM D882 |
Honeywell ACLAR® 11A(0.60 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |