Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.280 GPa | 40.6 ksi | ASTM D882 |
ExxonMobil Escorene® LD-108 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer high clarity film resin with a good balance of toughness, stiffness, and drawdown capability. This resin has good machinability in ba.. |
|||
Secant Modulus, TD | 0.280 GPa | 40.6 ksi | ASTM D882 |
ExxonMobil Escorene® LD-138 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin offering good clarity, toughness, and stiffness. Blown film made from this resin has good machinability in bag equipment a.. |