Mechanical Properties Metric English Comments
Secant Modulus, TD 0.130 GPa
18.9 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TS 7001 LDPE - Heavy Duty Low Friction Film
The Trithene TS 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and low coefficient of fricti..
Secant Modulus, TD 0.130 GPa
18.9 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TX 7001 LDPE - High Molecular Weight
The Trithene TX 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and environmental stress crac..
Secant Modulus, TD 0.130 GPa
18.9 ksi
ASTM D882
Chevron Phillips 7120ST LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene Copolymer, Cast/Blown Film ResinCharacteristics: Good Drawdown, Can be used in blown or cast applicationsApplications:Stretch Wrap, CoextrusionsProcessing Conditions: Extruder 6.3..
Secant Modulus, TD 0.130 GPa
18.9 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film
The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding..
Secant Modulus, TD 0.130 GPa
18.9 ksi
2% Secant Modulus; ASTM-D882
Braskem TS7010 LDPE Blown Film Extrusion Polyethylene
TS7010 is a low-density polyethylene (LDPE) that presents excellent processability and good mechanical properties. The incorporated additives package warrants a low coefficient of friction (COF) all..
Secant Modulus, TD 0.130 - 0.450 GPa
18.9 - 65.3 ksi
Average value: 0.253 GPa Grade Count:57
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m..
Secant Modulus, TD 0.130 GPa
18.9 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TS 3003 LDPE - Film Grade
The Trithene® TS 3003 resin is a low-density, high molecular weight polyethylene that offers high mechanical strength and excellent optical properties. The product shows high modulus of elasticity,..
Secant Modulus, TD 0.130 GPa
18.9 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TX 4003 LDPE and LLDPE Blend - High Resistance Film
The Trithene® TX 4003 resin is a blend of low-density polyethylene (LDPE) of high molecular weight with linear low-density polyethylene (LLDPE) designed for the production of industrial films. Sinc..