Mechanical Properties Metric English Comments
Secant Modulus, TD 0.0690 GPa
10.0 ksi
2% Secant; ASTM D882
Dow INTEGRALâ„¢ 906 Multilayer Adhesive Film
INTEGRAL 906 Adhesive Film is a heat-activated, thermally stable adhesive film capable of bonding to urethane foam-baked fabrics, polyester and nylon fabrics, fiberglass, and rigid urethanes.Informa..