Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.5557 GPa | 80.60 ksi | 2% Secant; ASTM D882 |
Dow Saran® 540 Vapor Retarder Film Saran™ Vapor Retarder Film is a biaxially oriented barrier film designed as a water vapor retarder for insulation applications. It is available in 400 gauge. Roll size: 35.5" x 375 long.Informat.. |