Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus, MD = 511 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 2.41 - 3.52 GPa
350 - 511 ksi
ASTM D882
Honeywell Capran® Emblem™ 1530 PVDC-Coated Bi-Axially Oriented Nylon Film  (discontinued **)
Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many ..
Secant Modulus, MD 2.41 - 3.52 GPa
350 - 511 ksi
ASTM D882
Honeywell Capran® Emblem™ 1500 Clear Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr..
Secant Modulus, MD 2.41 - 3.52 GPa
350 - 511 ksi
ASTM D882
Honeywell Capran® Emblem™ 1500M M-Coated Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd..
Copyright © lookpolymers.com All Rights Reserved