Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.2769 GPa | 40.16 ksi | 2% Secant; ASTM D882 |
Dow ELITE™ 5110G Enhanced Polyethylene Resin ™ 5110G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of high modulus and excellent impact strength, allowing for down gauging in bag applicatio.. |