Polymer Property : Secant Modulus, MD = 350 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 2.41 - 3.93 GPa
350 - 570 ksi
ASTM D882
Honeywell Capran® Emblem™ 1230 Bi-Axially Oriented Nylon Film  (discontinued **)
Description: Capran® Emblem™ 1230 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo..
Secant Modulus, MD 2.41 - 3.52 GPa
350 - 511 ksi
ASTM D882
Honeywell Capran® Emblem™ 1530 PVDC-Coated Bi-Axially Oriented Nylon Film  (discontinued **)
Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many ..
Secant Modulus, MD 2.41 - 3.55 GPa
350 - 515 ksi
ASTM D882
Honeywell Capran® Emblem™ 2530 Bi-Axially Oriented Nylon Film  (discontinued **)
Description: Capran® Emblem™ 2530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo..
Secant Modulus, MD 2.41 - 3.92 GPa
350 - 569 ksi
ASTM D882
Honeywell Capran® Emblem™ 1200 Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1200 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr..
Secant Modulus, MD 2.41 - 3.93 GPa
350 - 570 ksi
ASTM D882
Honeywell Capran® Emblem™ 1200MT Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1200MT is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hy..
Secant Modulus, MD 2.41 - 3.52 GPa
350 - 511 ksi
ASTM D882
Honeywell Capran® Emblem™ 1500 Clear Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr..
Secant Modulus, MD 2.41 - 3.52 GPa
350 - 511 ksi
ASTM D882
Honeywell Capran® Emblem™ 1500M M-Coated Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd..
Secant Modulus, MD 2.41 - 3.55 GPa
350 - 515 ksi
ASTM D882
Honeywell Capran® Emblem™ 2500 Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 2500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr..
Secant Modulus, MD 2.41 - 3.55 GPa
350 - 515 ksi
ASTM D882
Honeywell Capran® Emblem™ 2500M M-Coated Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 2500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd..
Secant Modulus, MD 2.41 GPa
350 ksi
ASTM D882
Total PPH 3271 Polypropylene, Oriented Film Extrusion Grade
Homopolymer film gradeLow Residuals – FINA 3271 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock –..
Secant Modulus, MD 2.41 GPa
350 ksi
ASTM D882
Total PPH 3371 Polypropylene, Oriented Film Extrusion Grade
Homopolymer film gradeLow Residuals - Fina 3371 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock - Fina..
Secant Modulus, MD 2.41 GPa
350 ksi
ASTM D882
Total PPH 3276 Polypropylene, Oriented Film Extrusion Grade
Homopolymer film gradeLow Residuals – Fina 3276 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock ..