Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.175 GPa | 25.4 ksi | ASTM D882 |
ExxonMobil Exceed™ 350D65 LDPE/Hexene Tough Premium Liner Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D65 resin have outstanding tensile, impact streng.. |
|||
Secant Modulus, MD | 0.175 GPa | 25.4 ksi | 1%; ASTM D882 |
Braskem LF 0720/20 AF LLDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Heavy duty bags; "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem |