Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 2.41 - 3.93 GPa | 350 - 570 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 1230 Bi-Axially Oriented Nylon Film
(discontinued **) Description: Capran® Emblem™ 1230 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo.. |
|||
Secant Modulus, MD | 2.41 - 3.52 GPa | 350 - 511 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 1530 PVDC-Coated Bi-Axially Oriented Nylon Film
(discontinued **) Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many .. |
|||
Secant Modulus, MD | 2.41 - 3.55 GPa | 350 - 515 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 2530 Bi-Axially Oriented Nylon Film
(discontinued **) Description: Capran® Emblem™ 2530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo.. |
|||
Secant Modulus, MD | 2.41 - 3.92 GPa | 350 - 569 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 1200 Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 1200 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr.. |
|||
Secant Modulus, MD | 2.41 - 3.93 GPa | 350 - 570 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 1200MT Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 1200MT is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hy.. |
|||
Secant Modulus, MD | 2.41 - 3.52 GPa | 350 - 511 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 1500 Clear Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 1500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr.. |
|||
Secant Modulus, MD | 2.41 - 3.52 GPa | 350 - 511 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 1500M M-Coated Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 1500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd.. |
|||
Secant Modulus, MD | 2.41 - 3.55 GPa | 350 - 515 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 2500 Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 2500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr.. |
|||
Secant Modulus, MD | 2.41 - 3.55 GPa | 350 - 515 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 2500M M-Coated Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 2500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd.. |
|||
Secant Modulus, MD | 2.41 GPa | 350 ksi | ASTM D882 |
Total PPH 3271 Polypropylene, Oriented Film Extrusion Grade Homopolymer film gradeLow Residuals – FINA 3271 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock –.. |
|||
Secant Modulus, MD | 2.41 GPa | 350 ksi | ASTM D882 |
Total PPH 3371 Polypropylene, Oriented Film Extrusion Grade Homopolymer film gradeLow Residuals - Fina 3371 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock - Fina.. |
|||
Secant Modulus, MD | 2.41 GPa | 350 ksi | ASTM D882 |
Total PPH 3276 Polypropylene, Oriented Film Extrusion Grade Homopolymer film gradeLow Residuals – Fina 3276 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock .. |