Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 1.310 - 1.551 GPa | 190.0 - 225.0 ksi | ASTM D882 |
Honeywell ACLAR® SupRx 900 CTFE Homopolymer, Barrier Film Description: ACLAR® SupRx 900 is a .9 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme.. |