Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.117 GPa | 17.0 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng.. |
|||
Secant Modulus, MD | 0.117 GPa | 17.0 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength.. |
|||
Secant Modulus, MD | 0.117 GPa | 17.0 ksi | ASTM D882 |
ExxonMobil Escorene® CR-5810 EVA Resin, for High Cling Stretch Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A tackified Ethylene Vinyl Acetate resin for blown or cast stretch film.Applications: Packing films (cling). Data for film properties below based o.. |
|||
Secant Modulus, MD | 0.117 GPa | 17.0 ksi | ASTM D882 |
Huntsman PE1501 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with excellent impact strength, good heat seal, and good clarity.Applications: Film extrusion: greenhouse film, heavy-duty packa.. |
|||
Secant Modulus, MD | 0.117 GPa | 17.0 ksi | ASTM D882 |
Huntsman PE1503 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Secant Modulus, MD | 0.117 GPa | 17.0 ksi | ASTM D882 |
Huntsman PE1504 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Secant Modulus, MD | 0.117 GPa | 17.0 ksi | ASTM D882 |
Huntsman PE1507 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Secant Modulus, MD | 0.117 GPa | 17.0 ksi | ASTM D882 |
Huntsman Rexell® V8402 Cast Film Extrusion LLDPE
(discontinued **) Ultra linear-low density copolymer, blown film extrusion, FDA compliant.Features: Excellent mechanical strength, low sealing temperature, and good flex crack resistanceApplications: Sealing layer in.. |
|||
Secant Modulus, MD | 0.117 - 0.420 GPa | 17.0 - 60.9 ksi | Average value: 0.218 GPa Grade Count:57 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m.. |
|||
Secant Modulus, MD | 0.117 GPa | 17.0 ksi | ASTM D882 |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |