Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.0900 GPa | 13.1 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TS 7045 LDPE - Film - Plastification The Trithene TS 7045 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |
|||
Secant Modulus, MD | 0.0900 - 0.390 GPa | 13.1 - 56.6 ksi | Average value: 0.196 GPa Grade Count:63 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum.. |
|||
Secant Modulus, MD | 0.0900 GPa | 13.1 ksi | 2% Secant; ASTM D882 |
Dow INTEGRAL™ 900 Deep Draw Multilayer Adhesive Film INTEGRAL 900 Adhesive Film is a heat-activated, moldable, thermally stable adhesive film capable of bonding to urethane foam-baked fabrics, polyester and nylon fabrics, fiberglass, and rigid urethan.. |