Polymer Property : Secant Modulus, MD = 0.280 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.280 GPa
40.6 ksi
ASTM D882
NOVA Chemicals Sclair® 14K1 Octene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer.
Secant Modulus, MD 0.280 GPa
40.6 ksi
ASTM D882
NOVA Chemicals Sclair® 14K3 Octene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer.
Secant Modulus, MD 0.280 GPa
40.6 ksi
ASTM D882
ExxonMobil Escorene® LD-117 MDPE Blown Overwrap Film Resin, Tough  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-117 can be used in overwrap applications and in push-through ..
Secant Modulus, MD 0.280 GPa
40.6 ksi
ASTM D882
ExxonMobil Escorene® LD-129 MDPE Cast Overwrap Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-129 can be used in overwrap applications and in push-through ..
Secant Modulus, MD 0.280 GPa
40.6 ksi
ASTM D882
DuPont™ Surlyn® 1650 Zinc Ionomer Resin for Blown and Cast Film
Surlyn® 1650 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
Secant Modulus, MD 0.280 - 0.450 GPa
40.6 - 65.3 ksi
Average value: 0.359 GPa Grade Count:15
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and..
Secant Modulus, MD 0.280 GPa
40.6 ksi
ASTM D882
DuPont™ Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film
Surlyn® 2601 is an ionomer resin available for use in blown and cast film operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins. Applicati..