Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.255 GPa | 37.0 ksi | ASTM D882 |
Chevron Phillips 7109BK Linear low density polyethylene blown film resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymer, blow film resin, medium slip, medium antiblock version of 7109Characteristics: good stiffness at thin gauges, good drawdown, low COF, c.. |
|||
Secant Modulus, MD | 0.255 GPa | 37.0 ksi | ASTM D882 |
Huntsman Rexell® M3104 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer, cast film extrusion, FDA compliant.Features: Excellent combination of toughness, stiffness, and optics with good temperature resistance.Applications: Diaper film.. |
|||
Secant Modulus, MD | 0.255 GPa | 37.0 ksi | 1% Strain; ASTM D882 |
M. Holland Company LL102 LLDPE
(discontinued **) Additives: Medium Antiblock, Medium SlipFeatures: Medium Antiblocking, Butene Comonomer, Copolymer, Good Drawdown, Good Processability, Medium SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c).. |
|||
Secant Modulus, MD | 0.255 GPa | 37.0 ksi | 1% Strain; ASTM D882 |
M. Holland Company LL106 LLDPE
(discontinued **) Additives: Antiblock, SlipFeatures: Unspecified Antiblocking, Hexane Comonomer, Copolymer, Good Drawdown, Good Processability, Unspecified SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.2.. |