Polymer Property : Secant Modulus, MD = 0.152 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.152 GPa
22.0 ksi
1% Secant; ASTM D882
Westlake Mxsten CV CV77515-F Plastomer  (discontinued **)
Mxsten CV plastomer CV77515-X is a polyethylene plastomer designed for blown film extrusion that contains medium slip and no antiblock additives. Films produced with this resin exhibit a very low s..
Secant Modulus, MD 0.152 GPa
22.0 ksi
ASTM D882
M. Holland Company LD219 LDPE  (discontinued **)
Features: Good Processability, Good ToughnessUses: Bottles, Industrial Applications, PackagingProcessing Method: Blow MoldingInformation provided by M. Holland.
Secant Modulus, MD 0.152 GPa
22.0 ksi
ASTM D882
M. Holland Company LD220 LDPE  (discontinued **)
Features: Good Heat Seal, Good Processability, Good ToughnessUses: Industrial Applications, Liners, PackagingProcessing Method: Blown FilmInformation provided by M. Holland.
Secant Modulus, MD 0.152 GPa
22.0 ksi
ASTM D882
ExxonMobil Escorene® LD-141 EVA Shrink Film Resin, FMI  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 2.0% vinyl acetate copolymer film resin with very good toughness and shrink properties. The low melt index gives excellent..
Secant Modulus, MD 0.152 GPa
22.0 ksi
ASTM D882
Huntsman PE1356 EVA Film Extrusion  (discontinued **)
3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
Secant Modulus, MD 0.152 GPa
22.0 ksi
ASTM D882
LyondellBasell Montell 16502F3 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA..
Secant Modulus, MD 0.152 GPa
22.0 ksi
ASTM D882
LyondellBasell Montell 16502F7 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet..
Secant Modulus, MD 0.152 GPa
22.0 ksi
ASTM D882
LyondellBasell Montell 16502F8 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee..
Secant Modulus, MD 0.152 GPa
22.0 ksi
1% Secant; ASTM D882
M. Holland Company LD220MM LDPE  (discontinued **)
Additives: Medium Antiblock, SlipFeatures: Medium Antiblocking, Good Heat Seal, Medium SlipUses: Liners, PackagingProcessing Method: Blown FilmInformation provided by M. Holland.
Secant Modulus, MD 0.152 - 0.208 GPa
22.0 - 30.2 ksi
Average value: 0.177 GPa Grade Count:4
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum ..
Secant Modulus, MD 0.152 GPa
22.0 ksi
ASTM D882
Huntsman PE1335 EVA Film Extrusion  (discontinued **)
3.3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
Secant Modulus, MD 0.152 GPa
22.0 ksi
ASTM D882
Huntsman PE1345 EVA Film Extrusion  (discontinued **)
3.4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
Secant Modulus, MD 0.152 GPa
22.0 ksi
ASTM D882
Huntsman PE 1375 EVA Film Extrusion  (discontinued **)
3.7% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
Secant Modulus, MD 0.152 GPa
22.0 ksi
1% Secant; ASTM D882
Westlake Hifor Xtreme SC74860-F Polyethylene  (discontinued **)
Hifor Xtreme Polyethylene SC74860-F is recommended for the core layer of cast stretch film. It provides excellent clarity and ultimate stretch values higher than the more conventional 2.0-2.5 MI cas..
Secant Modulus, MD 0.152 GPa
22.0 ksi
ASTM D882
Huntsman PE1353 EVA Film Extrusion  (discontinued **)
3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..