Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.140 GPa | 20.3 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® TF-0219-E Hexene LLDPE Film Resin Exceptional toughens, Low gel levelApplications: Cast stretch wrapAdditives: High temperature A/OFilm properties are typical of cast film extruded at a melt temperature of 540°F, and a line speed o.. |
|||
Secant Modulus, MD | 0.140 GPa | 20.3 ksi | ASTM D882 |
ExxonMobil Escorene® LD-315 EVA Packaging Film Resin for Frozen Food
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer clarity film resin. This resin's low melt index and its comonomer contact combine to provide film of special toughne.. |
|||
Secant Modulus, MD | 0.140 GPa | 20.3 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TN7006 LDPE Blown Film Extrusion Polyethylene TN7006 is a low-density polyethylene (LDPE) specially developed for coextruded films and lamination. The resin presents a great combination of mechanical, optical, and stiffness properties. TN7006 h.. |
|||
Secant Modulus, MD | 0.140 GPa | 20.3 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TS7003 LDPE Blown Film Extrusion Polyethylene TS7003 is a low-density polyethylene (LDPE) with high molecular weight that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily processed. Th.. |
|||
Secant Modulus, MD | 0.140 GPa | 20.3 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TS7006 LDPE Blown Film Extrusion Polyethylene TS7006 is a low-density polyethylene (LDPE) specially developed for coextruded films and lamination. The resin presents a combination of mechanical, optical, and stiffness properties. TS7006 has a l.. |
|||
Secant Modulus, MD | 0.140 GPa | 20.3 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TX7003 LDPE Blown Film Extrusion Polyethylene TX7003 is a low-density, high molecular-weight polyethylene that offers high mechanical strength. The product's characteristics allow for high versatility and use in various applications due to its .. |