Polymer Property : Secant Modulus, MD = 0.117 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.117 GPa
17.0 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film
The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng..
Secant Modulus, MD 0.117 GPa
17.0 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film
The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength..
Secant Modulus, MD 0.117 GPa
17.0 ksi
ASTM D882
ExxonMobil Escorene® CR-5810 EVA Resin, for High Cling Stretch Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A tackified Ethylene Vinyl Acetate resin for blown or cast stretch film.Applications: Packing films (cling). Data for film properties below based o..
Secant Modulus, MD 0.117 GPa
17.0 ksi
ASTM D882
Huntsman PE1501 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with excellent impact strength, good heat seal, and good clarity.Applications: Film extrusion: greenhouse film, heavy-duty packa..
Secant Modulus, MD 0.117 GPa
17.0 ksi
ASTM D882
Huntsman PE1503 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Secant Modulus, MD 0.117 GPa
17.0 ksi
ASTM D882
Huntsman PE1504 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Secant Modulus, MD 0.117 GPa
17.0 ksi
ASTM D882
Huntsman PE1507 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Secant Modulus, MD 0.117 GPa
17.0 ksi
ASTM D882
Huntsman Rexell® V8402 Cast Film Extrusion LLDPE  (discontinued **)
Ultra linear-low density copolymer, blown film extrusion, FDA compliant.Features: Excellent mechanical strength, low sealing temperature, and good flex crack resistanceApplications: Sealing layer in..
Secant Modulus, MD 0.117 - 0.420 GPa
17.0 - 60.9 ksi
Average value: 0.218 GPa Grade Count:57
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m..
Secant Modulus, MD 0.117 GPa
17.0 ksi
ASTM D882
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su..