Polymer Property : Secant Modulus, MD = 0.0900 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.0900 GPa
13.1 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TS 7045 LDPE - Film - Plastification
The Trithene TS 7045 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films..
Secant Modulus, MD 0.0900 - 0.390 GPa
13.1 - 56.6 ksi
Average value: 0.196 GPa Grade Count:63
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum..
Secant Modulus, MD 0.0900 GPa
13.1 ksi
2% Secant; ASTM D882
Dow INTEGRAL™ 900 Deep Draw Multilayer Adhesive Film
INTEGRAL 900 Adhesive Film is a heat-activated, moldable, thermally stable adhesive film capable of bonding to urethane foam-baked fabrics, polyester and nylon fabrics, fiberglass, and rigid urethan..