Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 9.10 MPa | 1320 psi | Lap |
Epoxy Technology EPO-TEK® H31 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H31 is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electronic.. |