Mechanical Properties Metric English Comments
Shear Strength 84.1 MPa
12200 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz..
Shear Strength 84.1 MPa
12200 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In..
Shear Strength 84.1 MPa

@Thickness 15.7 mm
12200 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP611 Paper Base Laminate
Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a..
Shear Strength 84.1 MPa
12200 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha..
Shear Strength 84.1 MPa
12200 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide..
Shear Strength 84.1 MPa
12200 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK)
KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha..
Shear Strength 84.1 MPa
12200 psi
Short Beam
Hexcel® HexPly® EH04 Epoxy Resin System, M35J Fiber
MS35J 120 24" EH04 31%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel
Shear Strength 84.1 MPa
12200 psi
Short Beam
Hexcel® HexPly® EH04 Epoxy Resin System, MS40 Fiber
MS40 120 24" EF04 31%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel
Shear Strength 84.1 MPa
12200 psi
Short Beam
Hexcel® HexPly® EH04 Epoxy Resin System, AS4C Fiber
AS4C 150 24" EH04 35%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel