Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 51.0 - 68.0 MPa | 7400 - 9860 psi | Average value: 58.2 MPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Shear Strength | 51.0 MPa @Temperature 80.0 °C |
7400 psi @Temperature 176 °F |
I.L.S. Warp, Wet; Pr EN 2563 |
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process. |