Polymer Property : Shear Strength = 70.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 70.3 MPa
10200 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte..
Shear Strength 70.3 MPa
10200 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and ..