Polymer Property : Shear Strength = 65.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 65.0 MPa

@Temperature 22.0 °C
9430 psi

@Temperature 71.6 °F
Hexcel® HexPly® 954-3 Curing Cyanate Resin, YSH-60A Fiber
Information provided by HexCel
Shear Strength 65.0 MPa
9430 psi
0°, Short Beam
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 315 g/m2
Information provided by HexCel
Shear Strength 65.0 MPa
9430 psi
0º, ILSS Short Beam, RT, Dry; EN2563
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon
Information provided by HexCel
Shear Strength 65.0 MPa
9430 psi
ILSS; EN2563
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/40%/285T2/AS4C-6K
Fiber: AS4C, Weave: 2x2T, 295 g/m2Information provided by HexCel
Shear Strength 65.0 MPa
9430 psi
ASTM D732
Ashley Polymers Ashlene® 528L Nylon 66
General purpose injection molding grade.Data provided by the manufacturer
Shear Strength 65.0 MPa
9430 psi
ASTM D732
Ashley Polymers Ashlene® 528LW Nylon 66
General purpose injection molding grade.Data provided by the manufacturer