Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Plaskolite Vivak PETG Sheet VIVAK offers a balance of physical properties and ease of fabrication. It is ideally suited for complex parts requiring fabrication, including deep thermoforming draws and precise molded-in details... |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Quadrant EPP Acetron® POM-H Homopolymer Acetal, Unfilled, Extruded (ASTM Product Data Sheet) |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Quadrant EPP Durapro® Truck Liners (ASTM Product Data Sheet) |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Quadrant EPP Quadrant PPSU LSG PPSU, Extruded, Unfilled, Polyphenylsulfone (ASTM Product Data Sheet) |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Quadrant EPP Techtron® 1000 PPS Extruded Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Quantum Polysulfone Information provided by Quantum Advanced Engineering Plastics |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Quantum PPS Information provided by Quantum Advanced Engineering Plastics |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Quantum PPSU Information provided by Quantum Advanced Engineering Plastics |
|||
Shear Strength | 62.1 MPa | 9010 psi | Conditioned; ASTM D732 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Quadrant EPP Quadrant LSG PSU, Extruded, Unfilled, Polysulfone (ASTM Product Data Sheet) |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Quadrant EPP Semitron® ESd 410C- CM Dissipative Polyetherimide(ASTM Product Data Sheet) |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Quantum Polycarbonate Information provided by Quantum Advanced Engineering Plastics |
|||
Shear Strength | 62.1 - 68.9 MPa | 9000 - 10000 psi | Average value: 63.4 MPa Grade Count:6 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Shear Strength | 62.1 - 75.8 MPa | 9000 - 11000 psi | ASTM D732 |
Mar-Bal MB2000-20 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Shear Strength | 62.1 MPa | 9010 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Spartech Polycast Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Spartech Polycast Poly 76 (Mil-P-8184) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Spartech Polycast Poly 84 (Mil-P-8184) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Spartech Polycast Poly 900 (DTD-5592-UK) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Spartech Polycast Poly II (Mil-P-5425) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Spartech Polycast UF3 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Spartech Polycast UF4 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Spartech Polycast UF96 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Spartech Polycast UVT (Ultra-Violet Transmitting) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Quadrant EPP Quadrant PSU Estruded Unfilled Polysulfone (ASTM Product Data Sheet) |
|||
Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
Quantum Acetal-Homopolymer Information provided by Quantum Advanced Engineering Plastics |
|||
Shear Strength | 62.1 - 101 MPa | 9010 - 14600 psi | Average value: 85.4 MPa Grade Count:17 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |