Mechanical Properties Metric English Comments
Shear Strength 32.4 MPa

@Temperature 23.9 °C
4700 psi

@Temperature 75.0 °F
Short-Beam, Dry; ASTM D2344
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 120 Aramid Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..
Shear Strength 32.4 MPa
4700 psi
Overlap, Distilled Water immersion for 30 days
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 32.4 MPa
4700 psi
Overlap, Water Vapor, 49°C at 100% RH for 30 days
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 32.4 MPa
4700 psi
Overlap, Etched Aluminum, 50% Antifreeze at RT for 30 days immersion, Cohesive Failure
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Shear Strength 32.4 MPa
4700 psi
Aluminum, etched, Overlap, 30 day IPA soak, Cohesive Failure
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f..
Shear Strength 32.4 MPa
4700 psi
Aluminum, etched, Overlap, 30 day IPA soak, Cohesive Failure
3M Scotch-Weld™ LSB60NS Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60NS is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of..
Shear Strength 32.4 MPa
4700 psi
Interlaminar S23; ASTM D2344
Polystrand ThermoPro™ IE7010 Unitape Unidirectional Polypropylene-Glass Composite
Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer ..