Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 3.05 MPa | 443 psi | |
Valley Adhesives EM-221 Low Temperature Application Glue Stick Valley Adhesives EM-221 Low Temperature Application Glue StickRapid strength build up to 0149; Excellent hot tack and wetting; Safe on styrofoam and heat sensitive materials; Bonds corrugated boxes .. |