Polymer Property : Shear Strength = 3630 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength >= 25.0 MPa
>= 3630 psi
ASTM D1002/DIN 53283
Palm Labs Adhesives Turbo Fuse Series 115SI Surface Insensitive (20 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 115SI – SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture...
Shear Strength >= 25.0 MPa
>= 3630 psi
Parallel to laminations; IEC 1212-2 5.6
Hippe PF CC 203 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet
Used in mechanical applications (fine weave: =130 g/m2, >30 threads/cm). Recommended for small parts. Better mechanical properties and poorer electrical properties than type PF CC 204.Information ..
Shear Strength >= 25.0 MPa
>= 3630 psi
Parallel to laminations; IEC 1212-2 5.6
Hippe PF CC 201 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet
Used in mechanical applications (coarse weave: >130 g/m2, =30 threads/cm). Better mechanical properties and poorer electrical properties than type PF CC 202.Information provided by Hippe.
Shear Strength >= 25.0 MPa
>= 3630 psi
wood; ASTM D1002/DIN 53283
BCC Products BC 100 Medium Cyanoacrylate Adhesive
BC100 Medium, like its name in the medium viscosity version of cyanoacrylate adhesive that has become most popular in the super bonding applications. A 12 second fixture bond makes the BC100 the fas..