Polymer Property : Shear Strength = 3025 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 20.86 MPa
3025 psi
after 30 days @ 49°C, 95-100% RH
3M Scotch-Weld™ EC-1469 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive EC-1469 is a one-part, 100% solids, thermosetting liquidInformation provided by 3M
Shear Strength 20.86 MPa
3025 psi
Overlap, Cold-Rolled Steel - solvent cleaned, Adhesive Failure
3M Scotch-Weld™ DP825 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP825 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..