Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 3.76 MPa | 545 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR III 3/8-5052-.005 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 3.76 MPa | 545 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.005 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 3.76 MPa | 545 psi | On Douglas Fir |
3M Scotch-Weld™ 3762 Hot Melt Adhesive Excellent “hot tack”, fast setting corrugated, beadboard, recouperage, repacking chipboard, wood and Economical, general purposeInformation provided by 3M |