Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 20.0 MPa | >= 2900 psi | Grit Blasted Steel; ASTM D1002/DIN 53283 |
Palm Labs Adhesives TURBO FUSE METHYL FOR METALS (75-95 Viscosity) Rapid Bonding Adhesive Palm Lab's Methyl Cyanoacrylate is a one component rapid bonding adhesive ideal for metal surfaces. TURBO FUSE METHYL’s advanced formula is designed to polymerize instantly by absorbing surface moi.. |
|||
Shear Strength | >= 20.0 MPa | >= 2900 psi | Stainless Steel; ASTM D1002/DIN 53283 |
Palm Labs Adhesives TURBO FUSE METHYL FOR METALS (75-95 Viscosity) Rapid Bonding Adhesive Palm Lab's Methyl Cyanoacrylate is a one component rapid bonding adhesive ideal for metal surfaces. TURBO FUSE METHYL’s advanced formula is designed to polymerize instantly by absorbing surface moi.. |
|||
Shear Strength | >= 20.0 MPa | >= 2900 psi | ASTM D1002/DIN 53283 |
Palm Labs Adhesives Turbo Fuse Series 115SI Surface Insensitive (20 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 115SI – SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture... |
|||
Shear Strength | 20.0 MPa | 2900 psi | |
Indium Corp. Indalloy 161 Lead Solder Alloy Torch solder, poor corrosion resistanceInformation Provided by Indium Corporation |
|||
Shear Strength | 20.0 - 30.0 MPa | 2900 - 4350 psi | in Plane |
Goodfellow Carbon-Carbon Composite Carbon Fiber - Carbon MatrixInformation provided by Goodfellow. |
|||
Shear Strength | 20.0 MPa @Temperature 175 °C |
2900 psi @Temperature 347 °F |
IL; After ageing at 70°C / 95% RH |
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix 5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel |
|||
Shear Strength | >= 20.0 MPa | >= 2900 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe PF CC 204 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications (fine weave: =130 g/m2, >30 threads/cm). Recommended for small parts.Information provided by Hippe. |
|||
Shear Strength | >= 20.0 MPa | >= 2900 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe PF CP 204 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in electrical and electronic applications. Good stability of electrical properties under high humidity. Also available in cold or hot-punching versions.Information provided by Hippe. |
|||
Shear Strength | >= 20.0 MPa | >= 2900 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe PF CP 205 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in electrical and electronic applications. Good stability of electrical properties under high humidity. Also available in cold or hot-punching versions. Flame retardant.Information provided .. |
|||
Shear Strength | >= 20.0 MPa | >= 2900 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe PF CP 206 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions.Information provided by Hippe. |
|||
Shear Strength | >= 20.0 MPa | >= 2900 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe SI GC 202 Woven Glass Cloth Reinforced Silicone Resin - Sheet Used in mechanical and electrical applications at elevated temperature. Good heat resistance.Information provided by Hippe. |
|||
Shear Strength | >= 20.0 MPa | >= 2900 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe UP GM 202 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant.Information provid.. |
|||
Shear Strength | >= 20.0 MPa | >= 2900 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe UP GM 204 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures.Information provided by Hippe. |
|||
Shear Strength | >= 20.0 MPa | >= 2900 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe UP GM 205 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures. Flame retardant.Information provided .. |
|||
Shear Strength | >= 20.0 MPa | >= 2900 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe EP GM 201 Glass Mat Reinforced Epoxy Resin - Sheet Used in mechanical and electrical applications. Extremely high mechanical strength at moderate temperature. Very good electrical properties under high humidity.Information provided by Hippe. |
|||
Shear Strength | >= 20.0 MPa | >= 2900 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe EP GM 203 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Shear Strength | >= 20.0 MPa | >= 2900 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe EP GM 204 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Shear Strength | >= 20.0 MPa | >= 2900 psi | grit blasted steel; ASTM D1002/DIN 53283 |
BCC Products BC 100 Medium Cyanoacrylate Adhesive BC100 Medium, like its name in the medium viscosity version of cyanoacrylate adhesive that has become most popular in the super bonding applications. A 12 second fixture bond makes the BC100 the fas.. |
|||
Shear Strength | 20.0 MPa | 2900 psi | CRS Overlap, Hydraulic Oil at RT |
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e.. |
|||
Shear Strength | 20.0 MPa | 2900 psi | Overlap, Aluminum; ASTM D1002-64 |
3M Scotch-Weld™ CA100 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. High-peel and impact strength and high thermal shock and heat resistance.Information provided by 3M.. |
|||
Shear Strength | 20.0 MPa | 2900 psi | Overlap, grit-blasted steel; ASTM D1002 |
3M Scotch-Weld™ MG300 FLX Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Shear Strength | 20.0 MPa | 2900 psi | Lap, Alum to Alum |
Atom Adhesives AA-BOND 428 Epoxy Adhesive AA-BOND 428 is a two part, heat-resistant and low exotherm, epoxy adhesive formulation. It is a 100% solid epoxy adhesive, with superior chemical resistance and shear strength. AA-BOND 428 contains .. |
|||
Shear Strength | 20.0 MPa | 2900 psi | Overlap, Aluminum -etched/oily |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 20.0 MPa | 2900 psi | Overlap, grit-blasted steel; ASTM D1002 |
3M Scotch-Weld™ MG100 SF Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Shear Strength | 20.0 MPa | 2900 psi | cured, grit-blasted steel; ASTM D1002 |
3M Scotch-Weld™ PR600 Plastic and Rubber Instant Adhesive 3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates .. |
|||
Shear Strength | 20.0 MPa | 2900 psi | cured, grit-blasted steel; ASTM D1002 |
3M Scotch-Weld™ SF100 Super Fast Instant Adhesive 3M™ Scotch-Weld™ Super Fast Instant Adhesives rely less on surface moisture for cure speed than standard cyanoacrylates. They are designed to join together difficult-to-bond plastics and rubbers, .. |
|||
Shear Strength | 20.0 MPa | 2900 psi | cured; ASTM D1002 |
3M Scotch-Weld™ SI5 Surface Insensitive Instant Adhesive 3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI5 (formerly SB20) is a very l.. |
|||
Shear Strength | 20.0 MPa | 2900 psi | Overlap, Galvanized Steel Hot dipped |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | >= 20.0 MPa | >= 2900 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe UP GM 203 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant. With improved re.. |
|||
Shear Strength | 20.0 - 74.0 MPa | 2900 - 10700 psi | Average value: 39.9 MPa Grade Count:15 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |