Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 28.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 28.3 MPa

@Temperature 23.9 °C
4100 psi

@Temperature 75.0 °F
Short Beam; Dry; ASTM D790
Park Electrochemical Nelcote® V-303 Polyimide Prepreg, 7781 E-Glass Reinforced
Nelcote® V-303 is non-MDA condensation polyimide prepreg with a service temperature of 600°F.Key Features and Benefits:600°F maximum service temperatureGood electrical properties for RF applicati..
Shear Strength 28.3 MPa
4100 psi
Overlap, Brass MEK/abrade/MEK
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 28.3 MPa
4100 psi
Overlap, Aluminum - abraded, 150 grit sandpaper, Adhesive Failure
3M Scotch-Weld™ DP807 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Shear Strength 28.3 MPa
4100 psi
Overlap, Etched Aluminum tested after 1 week of Immersion in IPA
3M Scotch-Weld™ DP807 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Shear Strength 28.3 MPa
4100 psi
Overlap, Bare Aluminum, Cohesive Failure
3M Scotch-Weld™ DP810NS Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 28.3 MPa
4100 psi
Overlap, Aluminum, Cohesive Failure
3M Scotch-Weld™ DP8405NS Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP8405NS is a high performance, two-part acrylic adhesives that offer excellent shear, peel and impact performance. These toughened adhesives provide improved adh..
Shear Strength 28.3 MPa
4100 psi
Overlap, Aluminum - bare, Adhesive Failure
3M Scotch-Weld™ DP825 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP825 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Shear Strength 28.3 MPa
4100 psi
Aluminum, etched, Overlap, 30 day Gasoline soak, Cohesive Failure
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f..