Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 220 MPa | 31900 psi | ASTM D732 |
Performance Polymers IPS II PPL-C4150 PEKK (Polyetherketoneketone) Linear 30 % Glass Fiber Reinforced Molding Grade Amber pelletsInformation provided by Infinite Polymer System II. |
|||
Shear Strength | 220 MPa | 31900 psi | |
Indium Corp. Indalloy 184 Gold Solder Alloy Information Provided by Indium Corporation |