Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 20.86 MPa | 3025 psi | after 30 days @ 49°C, 95-100% RH |
3M Scotch-Weld™ EC-1469 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1469 is a one-part, 100% solids, thermosetting liquidInformation provided by 3M |
|||
Shear Strength | 20.86 MPa | 3025 psi | Overlap, Cold-Rolled Steel - solvent cleaned, Adhesive Failure |
3M Scotch-Weld™ DP825 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP825 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |