Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 19.7 MPa | 2850 psi | Overlap, CRS/CRS after 7 days of Immersion in Machine Oil |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 19.7 MPa | 2850 psi | Overlap at 1 hr after bonding |
3M Scotch-Weld™ DP810NS Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 19.7 MPa | 2850 psi | Etched Aluminum Overlap, 100% RH @ 49°C for 356 days |
3M Scotch-Weld™ EC-2086 Structural Adhesive 3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M |
|||
Shear Strength | 19.7 MPa | 2850 psi | Overlap, Steel, Adhesive Failure |
3M Scotch-Weld™ Thick Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Shear Strength | 19.7 MPa | 2850 psi | Overlap, Steel, Adhesive Failure |
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Shear Strength | 19.7 MPa @Temperature -53.0 °C, Time 0.000 sec |
2860 psi @Temperature -63.4 °F, Time 0.000 hour |
Overlap, Cured for 7 days at 24°C |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |