Mechanical Properties Metric English Comments
Shear Strength 8.62 - 11.0 MPa
1250 - 1600 psi
ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works.
Shear Strength 9.65 - 11.0 MPa
1400 - 1600 psi
ITW Plexus Plexusâ„¢ MA1023 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works.
Shear Strength 8.96 - 11.0 MPa
1300 - 1600 psi
ITW Plexus Plexusâ„¢ MA420FS Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, very fast curing.Information provided by Illinois Tool Works.