Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 108 MPa | 15700 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Shear Strength | 108 MPa | 15700 psi | ASTM D732 |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon PAI grades cannot be molded successfully in molds with undercuts. Torlon 4601 has been formulated to be moldable.. |
|||
Shear Strength | 108 MPa | 15700 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Shear Strength | 108 MPa | 15700 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Shear Strength | 108 MPa | 15700 psi | ASTM D732 |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI) Torlon® 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon® PAI grades cannot be molded successfully in molds with undercuts. Torlon® 4601 has been formulated to.. |
|||
Shear Strength | 108 MPa | 15700 psi | In-Plane, RT, Dry; EN6031 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 54%/G1088 Glass/Carbon Fiber Information provided by HexCel |
|||
Shear Strength | 108 MPa | 15700 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |